top.jpg (17743 bytes)
l1.jpg (7163 bytes)Company ProfileProductsTest Procedures
l2.jpg (6093 bytes)Material Testing ManualFeedback

PLASTER OF PARIS


Plaster of paris is manufactured by heating gypsm at 120o - 160oC. When Plaster of Paris is mixed in water it rehydrates and form dense matrix of gypsm crystal.


Chemical Formula : CaSO4, 1/2H2O

Typical Chemical Analysis :

SiO : 0.94%
Fe2O3 : 0.28%
Al2O3 : 0.69%
CaSO4, 1/2H2O : 97.97%
MgO : 00.12%

Applications : Plaster of Paris forms the basis of many commercial, Plasters used for interior decoration. As a false cieling, studio sets etc.


Normal Supplies : 240 mesh only.

Packing : HDPE 25/40 Kgs. nett.


Go Directly :

 

Image Map